Environmental Gaseous Contamination NOTE: Maximum corrosive contaminant levels measured at ≤50% relative humidity. Copper Coupon Corrosion Rate Silver Coupon Corrosion Rate
![](/manual_guide/products/dell-powervault-dr6000-getting-started-guide-a62b9e4/9.png)
Environmental
Gaseous Contamination
NOTE:
Maximum corrosive contaminant levels measured at ≤50% relative humidity.
Copper Coupon Corrosion Rate
<300 Å/month per Class G1 as defined by ANSI/
ISA71.04-1985.
Silver Coupon Corrosion Rate
<200 Å/month as defined by AHSRAE TC9.9.