Brother International BAS-341F Instruction Manual - English - Page 60

Notes On The Processing And Production Of Plate Blanks

Page 60 highlights

14.NOTES ON THE PROCESSING AND PRODUCTION OF PLATE BLANKS 14. NOTES ON THE PROCESSING AND PRODUCTION OF PLATE BLANKS Plate blank After processing Plate blank After processing 1968S * Chamfer other corners of the reverse side of the plate blank with a thickness of C0.3 or thicker, and finish the corners with fine sand paper. Please carry out the following points to chamfer the reverse side of the plate blank when using the plate blank for any supplementary processing of material. *Cross-section A-A' Use fine sand paper or similar material to acquire a smooth surface for this section. 1969S Point at which to use sand paper, etc. 1970S BAS-341F, 342F 53

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8
  • 9
  • 10
  • 11
  • 12
  • 13
  • 14
  • 15
  • 16
  • 17
  • 18
  • 19
  • 20
  • 21
  • 22
  • 23
  • 24
  • 25
  • 26
  • 27
  • 28
  • 29
  • 30
  • 31
  • 32
  • 33
  • 34
  • 35
  • 36
  • 37
  • 38
  • 39
  • 40
  • 41
  • 42
  • 43
  • 44
  • 45
  • 46
  • 47
  • 48
  • 49
  • 50
  • 51
  • 52
  • 53
  • 54
  • 55
  • 56
  • 57
  • 58
  • 59
  • 60
  • 61
  • 62
  • 63
  • 64
  • 65
  • 66
  • 67

14.NOTES ON THE PROCESSING AND PRODUCTION OF PLATE BLANKS
BAS-341F, 342F
53
14.
NOTES ON THE PROCESSING AND
PRODUCTION OF PLATE BLANKS
*
Chamfer other corners of the reverse side of the plate blank with a thickness of C0.3 or thicker, and finish the corners
with fine sand paper.
Please carry out the following points to chamfer the reverse side of the plate blank when using the plate blank for any
supplementary processing of material.
Plate blank
After processing
1968S
*Cross-section A-A’
Use fine sand paper
or similar material
to acquire a smooth
surface for this section.
Point at which to use
sand paper, etc.
1969S
1970S
Plate blank
After processing