Ricoh FAX2210L Operating Instructions - Page 176
Category, Specifications, Symptom, Problem with Paper, Solution, certain types of thermography.
UPC - 026649304705
View all Ricoh FAX2210L manuals
Add to My Manuals
Save this manual to your list of manuals |
Page 176 highlights
Symptom Problem with Paper Excessive curl problems with Too moist, wrong grain feeding direction or short-grain construction Jamming, damage to machine Cutouts or perforations Problems with feeding Ragged edges Solution • Use the rear output slot. • Use long-grain paper. Do not use paper with cutouts or perforations. Use good quality paper. NOTES: • Do not use letterhead paper printed with low-temperature inks, such as those used in certain types of thermography. • Do not use raised or embossed letterhead. • The machine uses heat and pressure to fuse toner to the paper. Insure that any colored paper or preprinted forms use inks that are compatible with this fusing temperature (200 °C or 392 °F for 0.1 second). Paper Specifications Category Acid Content Caliper Curl in Ream Cut Edge Conditions Fusing Compatibility Grain Moisture Content Smoothness Specifications 5.5 pH or lower 0.094 ~ 0.18 mm (3.0 ~ 7.0 mils) Flat within 5 mm (0.02 in.) Cut with sharp blades with no visible fray. Must not scorch, melt, offset or release hazardous emissions when heated to 200 °C (392 °F) for 0.1 second. Long Grain 4 % ~ 6 % by weight 100 ~ 400 Sheffield A A.11